DIN EN ISO 4957
1.3343 HS 6-5-2
AISI /SAE JIS GB
M2 SKH9 W6Mo5Cr4V2
Chemical Composition
C% | Si% | Mn% | P%≤ | S%≤ | Cr% | Mo% | V% | W% |
0.86-0.94 | ≤0.45 | ≤0.40 | 0.03 | 0.02 | 3.8-4.5 | 4.7-5.2 | 1.7-2.0 | 6.0-6.7 |
Steel Properties
Molybdenum high speed tool steel.Very high resistance to softening at elevated temperatures.Very high resistance to wear.Good toughness and cutting capability.Deep hardening response.
Applications
Knives.thread cutting and twist drills,broaching and milling tools,woodworking tools,cold working tools,sendzimir rolls.
Heat Treatment
Annealing: 790 – 820 °C
Hardening:: 1190 – 1230 °C
Tempering: 550- 570 °C
In laoreet augue vel volutpat elementum. Quisque
Contact: Michael
Phone: +86-15997138795
Tel: +86-15997138795
Email: michael@hswinningsteel.com
Add: NO.14-1-1-403,YINGBIN AVENUE, HUANGSHIGANG DISTRICT, HUANGSHI, HUBEI,P.R.CHINA