DIN EN ISO 4957
1.2365 32CrMoV12-28
AISI /SAE GOST GB
H10 3X3М3Ф 4Cr3Mo3SiV
Chemical Composition
C% | Si% | Mn% | P%≤ | S%≤ | Cr% | Mo% | V% |
0.28-0.35 | 0.10-0.40 | 0.15-0.45 | 0.030 | 0.020 | 2.70-3.20 | 2.50-3.00 | 0.40-0.70 |
Steel Properties
Excellent wear resistance and toughness at high temperatures. Good machinability in annealed condition. Good polishability. Good hardenability. Very good dimensional stability. Excellent tempering resistance.
Applications
Dies, tools for the production of screws and forging machines, highly stressed extruding tools for light metal processing-mandrels, pressing die cast molds.
Heat Treatment
Annealing: 760 – 780 °C
Stress Relief Annealing: 600 - 650°C
Hardening:: 1010 – 1030 °C
Tempering: 540 – 560 °C